We now have many fantastic staff members customers superior at advertising, QC, and working with varieties of troublesome problem within the generation system for Well-designed Redispersible Polymer Emulsion Powder White Construction Rdp, All costs depend upon the quantity of your respective order; the additional you order, the extra economical the cost is. We also offer good OEM assistance to numerous famous brands.
We now have many fantastic staff members customers superior at advertising, QC, and working with varieties of troublesome problem within the generation system for CAS 24937-78-8, Cement Additives, China Rdp, China Vae, Ethylene-vinyl acetate copolymer, Redispersible Polymer Powder, Redispersible Rubble Powder, Furthermore, all of our products are manufactured with advanced equipment and strict QC procedures in order to ensure high quality. If you are interested in any of our products, please don’t hesitate to contact us. We will do our best to meet your needs.
Introduction
RDP 2000 improves adhesion, flexural strength, abrasion resistance and workability of modified compounds such as tile adhesives, self-leveling compounds and gypsum based compounds. It is therefore compatible with mortar additives used to achieve special processing characteristics.
RDP 2000 contains a fine, mineral filler as anti-block agent. It is free of solvents, plasticizers and film-forming aids.
Indicators
Product Specifications
Solid Content | >99.0% |
Ash content | 10±2% |
Appearance | White Powder |
Tg | 5℃ |
Typical Proerty
Polymer Type | VinylAcetate-Ethylene copolymer |
Protective Colloid | Polyvinyl Alcohol |
Bulk Density | 400-600kg/m³ |
Average Particle Size | 90μm |
Min Film Forming Temp. | 5℃ |
pH | 7-9 |
Construction:
1.0Exterior Thermal Insulation System(EIFS)
Tile Adhensive
2. Grouts/Joint Mixture
3. Binding Mortar
4.Water-proofing/Repairing Mortars
Package&Storage:
Package: 25kg paper plastic bags with PP liner. Alternative package may be available upon request.
Storage: Shelf-life time is 1 year if kept in cool, dried place.Test should be done after expiration.